    分析环氧树脂耐磨地坪漆常见质量问题

    2018-11-06 08:32:42 无锡盛发地坪科技有限公司 阅读

    环氧树脂耐磨地坪漆有着防腐蚀、耐磨损、防滑、污染小及装饰性强等特点,在工业环氧地坪及环境要求场所所得到了大量采用,由于施工质量和环境因素的影响导致产生一些质量问题,下面就环氧树脂耐磨地坪漆常见问题做个分析:在选购环氧地坪漆商家尤为重要,市场上呈现大量劣质环氧地坪漆生产厂家,施工技术不到位,都是导致以上问题出现的源头。

    Epoxy resin wear-resistant floor paint has the characteristics of corrosion resistance, wear resistance, skid resistance, small pollution and strong decoration. It has been widely used in industrial epoxy floor and environmental requirements places. Due to the influence of construction quality and environmental factors, some quality problems have arisen. Here are some common problems of epoxy resin wear-resistant floor paint. An analysis: It is particularly important to select and purchase epoxy floor paint manufacturers. A large number of inferior epoxy floor paint manufacturers and inadequate construction technology are the sources of the above problems. 1、渗色问题

    1. The problem of colouring.

    渗色是指当一种颜色底漆涂膜上覆盖另一种颜色的面漆时,会让表面涂膜出现变色的情况,主要原因有以下几点:底漆并没有完全干燥、底漆和面漆颜色上有色差、漆中含有杂色物质。

    Colouring refers to the discoloration of the surface coating when one color primer is coated with another color. The main reasons are as follows: the primer is not completely dry, the color of the primer and the top coat is different, and the paint contains impurities.

    2、漆面较花

    2. The paint is more beautiful.

    是指涂膜表面色彩不够均匀,有斑纹及颜色杂乱的现象,原因是由于施工过程中,涂脸的配料不当及涂抹不均匀所致。

    It refers to the phenomenon that the color of the coating surface is not uniform enough, there are spots and disorderly colors. The reason is due to improper ingredients and uneven application during the construction process.

    3、表面泛白

    3. Surface whitening

    是指施工作业完成后,地表涂层的涂抹出现泛白现象,原因有几点:空气中的湿度过高、涂面干燥过程使用了过多的快干剂。

    It refers to the whitening phenomenon of surface coating after the completion of construction work. There are several reasons: excessive humidity in the air, excessive use of quick drying agent in the drying process of coating surface.

    4、起皱、针眼、鱼眼

    4. Wrinkle, needle eye, fish eye.

    涂膜表层出现起皱现象,主要原因是漆面内外层干燥速度不一致造成表层收拢起皮、针眼是因为溶剂发挥太快,漆液补充不及时造成的、鱼眼是因为涂料或外界的杂质混入造成涂料附着力不均匀。

    The wrinkling phenomena on the surface of coatings are mainly caused by the inconsistency of drying speed between the inner and outer layers of the coatings, which results in the folding up of the surface and pinholes because the solvent is exerted too fast, the filling of the paint is not timely, and the fisheye is due to the uneven adhesion of the coatings caused by the mixing of paint or external impurities.

    5、粗糙、开裂问题

    5. Rough and cracked problems

    粗糙现象是指表层有大小不同的颗粒状物质出现,主要原因是涂料中含有不易溶解的杂质及外界灰尘所致。地表开裂现象是因为原材料和施工质量问题,导致漆层附着力下降,在外界作用力影响下,出现掉皮开裂现象。

    Roughness refers to the appearance of granular substances of different sizes on the surface. The main reason is that the coating contains insoluble impurities and external dust. Surface cracking is caused by quality problems of raw materials and construction, which leads to the decrease of adhesion of paint layer. Under the influence of external forces, skin cracking occurs.