    地坪厂家对新建或翻新环氧地坪漆起皮怎么处理?

    2018-11-02 07:11:53 无锡盛发地坪科技有限公司 阅读

    环氧地坪有着众多的优点于一身,是其他地面材料无法比拟的,在众多领域广泛使用,任何产品都有寿命,环氧地坪也不例外,再加上现在劣质环氧地坪漆、偷工减连、基层缺陷等加速使环氧地坪出现各种问题,最常见的如起皮、起泡、发白发花等。造就了在使用环氧地坪漆场所中多次翻新或修补。

    Epoxy flooring has many advantages, which are incomparable with other flooring materials. It is widely used in many fields. Every product has a life span. Epoxy flooring is no exception. With the acceleration of inferior flooring paint, jerry-building and grass-roots defects, all kinds of problems arise in epoxy flooring, such as peeling, etc. Blistering, whitish and flowers. It has been renovated or repaired many times in the use of epoxy floor paint. 

    那么我们就拿各行业的生产车间、厂房环氧地坪最容易出现的起皮脱层的情况,怎么解决。所谓的起皮脱层即基层或环氧底涂失去应有的附着力,在外力的作用下导致环氧涂层脱离。航特的项目部老员工告诉大家,把控三点:环氧地坪漆材料、工艺和人员、基材。不论是新建或环氧地坪翻新都能让其寿命真正的耐用长久。

    Then we will take the most vulnerable situation of peeling and delamination of epoxy flooring in production workshops and factories of various industries, and how to solve it. The so-called peeling delamination means that the base or epoxy primer loses its proper adhesion, which leads to the separation of the epoxy coating under the action of external forces. Aircraft Project Department veteran staff told you that the control of three points: floor paint materials, technology and personnel, base materials. No matter new or epoxy floor refurbishment can make life long and durable.

    环氧地坪

    地坪漆材料:环氧地坪漆本身成膜特性,劣质的地坪漆树脂含量太低,基层或者底中面各图层涂层附着力效果不良。施工用量及搅拌配比控制等。

    Material of floor paint: Epoxy floor paint has film-forming characteristics. The resin content of inferior floor paint is too low, and the adhesion effect of base or middle layer coating is poor. Construction dosage and mixing ratio control.


    工艺和人员:按照环氧地坪漆特性及业主对地面功能性定制施工工艺,并且每道工艺完成要检查过程监督,符合条件在进行下一道工艺施工;选择专业的施工队伍,在施工时技术发挥将凸显及影响完工后地坪质量等。

    Technologies and personnel: According to the characteristics of epoxy floor paint and the owner's customized construction technology for the floor function, and each process should be inspected and supervised to meet the requirements for the next process construction; select professional construction team, in the construction of technology will highlight and affect the quality of the floor after completion.

    环氧地坪

    基材:基层的抗压强度,含水率,混凝土C25以上标号,不去沙。基层整体研磨不佳等都是环氧地坪起皮的致命伤。旧地面翻新必须清除表面上的油污、蜡、积水和化学药品等。

    Substrate: compressive strength, moisture content of the base, concrete C25 above label, not sand. Poor grinding at the grassroots level is the fatal wound of the epoxy floor. Old surface refurbishment must remove oil, wax, water and chemicals on the surface.

    1934年德国I.G.Farben公司的P.Schlack发展地坪漆的环氧合物可以固化,生成低收缩率的塑料而取得瑞士专利。随后开始应用于环氧树脂地坪漆的地面使用;标示着环氧树脂地坪的正式诞生。

    In 1934, P. Schlack of I. G. Farben developed a Swiss patent for the curing of epoxy compounds in floor paints to produce plastics with low shrinkage. Then it began to be used on the ground of epoxy floor paint, marking the formal birth of epoxy floor paint.



    标签:   环氧地坪 地坪 环氧地坪翻新 环氧地坪施工 环氧地坪漆
    无锡环氧地坪 技术支持:【易商科技】