    环氧地坪冬季最常见的龟裂问题,是因为环氧耐磨地坪漆厂家在进行施工中,施工间隔过短,环氧地坪漆不配套,环氧地坪漆涂层之间过厚或者因为材料搅拌不均匀等原因所导致的,其实造成龟裂问题出现的原因在专业的地坪漆施工师傅手中都是可以成功避免的,其中最主要的是在施工前和施工中做好预防措施。

    The most common cracking problem of epoxy floor in winter is caused by the short construction interval, incomplete floor paint, excessive thickness between floor paint coatings or uneven mixing of materials in the construction of epoxy wear-resistant floor paint manufacturers. In fact, the causes of cracking problem are professional floor paint builders. Fuzhong can be successfully avoided, the most important is to do a good job in the construction of precautions before and during the construction. 在冬季低温下,地坪漆接触混凝土被冷却,反应热及时散发,会使固化时间变长,而环氧地坪漆固化时间变长就会使得涂层施工之间的间隔需要延长,而有些环氧耐磨地坪漆厂家为了赶进度,没有等底漆干透就贸然进行第二涂层的施工,最后导致两层涂膜内外伸缩力不一致导致开裂。在地坪漆施工过程中,一定要把握好每层环氧地坪漆的厚度,尤其在冬季低温下,地坪涂料的固化时间长,过厚的地坪材料越难干。 对于已经有龟裂现象的地坪地面也要分情况进行修复,只是轻微龟裂的地面,在保证材料不冲突的情况下,再滚涂一遍面漆覆盖就可以了,而有明显裂纹的龟裂现象,就需要环氧耐磨地坪漆厂家先用环氧中涂进行填充修补再滚涂一遍面漆。

    At low temperatures in winter, floor paint contact with concrete is cooled, and the reaction heat is released in time, which will make the curing time longer, while the curing time of epoxy floor paint will make the interval between coating construction needs to be extended, and some epoxy wear-resistant floor paint manufacturers in order to catch up with the progress, without waiting for the primer to dry through the second coating. The construction of the layer finally leads to the two layers of paint film internal and external expansion force inconsistency leading to cracking. In the process of floor paint construction, we must grasp the thickness of each layer of epoxy floor paint, especially in winter low temperature, the floor paint solidification time is long, the thicker the floor material is more difficult to dry. For the ground that has cracks, it should be repaired according to different conditions. Only slightly cracked ground can be repaired by rolling over the top coat once more under the condition of guaranteeing no conflict of materials. Coat the top coat.


    标签:   环氧地坪 地坪 环氧地坪漆 环氧地坪施工
    无锡环氧地坪 技术支持:【易商科技】