    如何解决环氧地坪漆涂膜表面粗糙和漆膜肿胀的问题

    2018-10-31 18:50:38 无锡盛发地坪科技有限公司 阅读

    环氧地坪漆涂装出现粗糙的现象主要以下四点:1、由于施工环境不洁净,有较多的灰尘,灰尘黏在涂膜上就会出现粗糙;2、不过滤环氧地坪漆涂料,使杂质混入里边,当涂膜干燥以后就会在环氧地坪上显示出来;3、由于涂料开端胶化仍然连续施工,由于环氧地坪漆都是双组分的,加入固化剂以后就会发生化学反应,然后固化成魔,假如那时光还在施工就会以致粗糙;4、施工现场的温度太高,使得稀释剂蒸发速度快,环氧地坪漆还不流平就现已固化。

    Epoxy floor paint coating appears roughness of the following four main points: 1, because the construction environment is unclean, there is more dust, dust will appear roughness sticking to the film; 2, but filter epoxy floor paint, so that impurities mixed inside, when the film drying will be displayed on the floor; 3, because the paint began; Gelatinization is still continuous construction, because the epoxy floor paint is a two-component, after adding curing agent will occur chemical reaction, and then cured into a magic, if the time is still in the construction will result in rough; 4, the construction site temperature is too high, so that the thinner evaporation speed, epoxy floor paint is not leveling has been cured. 由于丙烯酸树脂环氧地坪漆色浅、耐候、保色、快干和有一定的耐腐蚀性。这些年,常造成单组分常温型木器家私漆。在地坪漆涂装过程中,这类漆也常出现漆膜肿胀,漆膜不平坦、光芒不平均、渗色、漆膜起皱、漆膜色包、发花等天气。

    Because acrylic resin floor paint is light, weather resistant, color fast drying and has certain corrosion resistance. These years often result in one component, normal temperature wooden furniture. In the process of painting floor paint, this kind of paint often appears film swelling, film uneven, uneven light, color infiltration, film wrinkling, film color bag, blossom and other weather.

    环氧地坪漆涂装工作时,未干的漆膜遭到淋雨,或在湿润的底材上涂漆,底层漆与面漆不配套,漆膜遭到酸碱和热的感化是引起漆膜肿胀的要素。

    When the epoxy floor paint is applied, the wet substrate or the wet film is coated. The underlying paint does not match the top coat, and the film is affected by acid, alkali and heat.

    涂装地坪漆膜干燥后,底漆分开基底拱起或面漆分开底漆拱起,里边有气体或液体,呈不平均散布。

    After drying the coating film, the primer is separated from the base arch or the topcoat is separated from the primer arch, with gas or liquid inside, which is unevenly distributed.

    要严厉执行底材干燥和名义处理的环氧地坪漆涂装规矩,在腻子或漆膜完整干燥的情形下再施工涂装。地坪漆涂装时,要用无传染的抹布抹漆膜或用干燥空气喷吹漆膜一遍,以去掉水汽或微节露水才施工。要选择配套腻子和配套底漆,忌用虫胶底漆和酸固化底漆。

    Strict enforcement of the substrate drying and nominal treatment of epoxy floor paint painting rules, in the putty or film in the case of complete drying re-construction coating. Floor paint painting, to use non-contagious cloth paint film or dry air spray paint film again, to remove water vapor or dew before the construction. It is necessary to choose matching putty and matching primer, avoid using insect base paint and acid curing primer.

    处理环氧地坪漆涂装出现粗糙的办法:

    The rough way to treat epoxy floor paint is:

    1、在施工环氧地坪漆之前一定要将施工现场扫除洁净,将涂料按照身分分配好,然后用120目纱布把涂料过滤以后再施工。

    1. In the construction of epoxy floor paint must be cleaned before the construction site, the paint according to identity distribution, and then use 120 mesh gauze to filter the paint after the construction.

    2、施工前要根据施工时光核算涂料的用量,再停止涂料配比和浓缩的工作。不克不及多配,使用的稀释剂需要慢干的高飞点的。

    2, before construction, the amount of paint should be accounted for according to the construction time, and the proportion and concentration of paint should be stopped. It can't be matched with the thinner. It needs slow dry high flying points.

    3、处理好上层,从底层开端就要按施工请求做好,中层要根绝粗糙天气,面层施工前一定要把中层整理洁净,否定无灰尘后再施工,这么就能够处理环氧地坪漆该类的粗糙天气了.

    3. Processing the upper layer well, starting from the bottom, we should do a good job according to the construction requirements, the middle layer to eradicate rough weather, surface construction must be cleaned up before the middle layer, deny dust-free construction, so that we can deal with epoxy floor paint this kind of rough weather.

    地坪漆漆膜出现肿胀后,只能把已出现成绩的漆膜打磨去掉,选择底面漆配套的二道底漆涂装干燥后,再从头涂装面漆

    When the film of floor paint becomes swollen, only the film that has already achieved good results can be polished off. Choose two primers matched with primers to dry, and then apply top coat from scratch.