    环氧地坪漆涂装之后,要经过固化而成膜,进而形成光滑耐用的环氧地坪。根据资料显示,环氧地坪漆的固化的时间以及成膜后的质量大多都不相同,这是因为影响环氧地坪漆固化的因素有很多,包括主观的因素和可观的,任何一个方面的因素都决定着它固化成膜的时间和质量。那么,影响环氧地坪漆固化成膜的因素有哪些呢?根据总结,主要有以下四个方面:

    After coating the epoxy floor paint, it must be cured to form a smooth and durable epoxy floor. According to the data, the curing time and quality of the epoxy floor paint are mostly different, because there are many factors affecting the curing of the epoxy floor paint, including subjective factors and considerable, any one of the factors determines the curing time and quality of the film. Then, what are the factors that affect the epoxy floor paint curing film formation? According to the summary, there are four main aspects: 1、环氧地坪漆涂料对基础质量、底漆材料的附着力和渗透性的性能要求较高,环氧地坪漆底漆材料与基础地面的粘接效果是决定固化成膜后的环氧地坪工程的质量和性能发挥的关键。

    1. Epoxy floor coatings require high base quality, adhesion and permeability of primer materials. The bonding effect between primer materials and base floor is the key to the quality and performance of cured epoxy floor coatings.

    2、客观因素中基础质量强度和表面接触面的粗糙程度能提升底漆材料与基础的附着力,环境的温度和湿度以及施工场所的通风条件及底材清洁度,会影响环氧地坪漆固化时间和固化后涂层的质量。

    2. The base quality strength and roughness of the surface contact surface of the objective factors can enhance the adhesion of the primer material to the foundation, the temperature and humidity of the environment, the ventilation conditions of the construction site and the cleanliness of the base material, which will affect the curing time of the floor paint and the quality of the cured coating.

    3、施工涂层的厚度是涂层与涂层之前,涂装间隔时间;干燥固化时间(表干、硬干),材料配比(环氧树脂与固化剂)的标准性会影起涂层不干(没加固化剂或者加入的固化剂量少的情况)。

    3. The thickness of the coating is the interval time between coating and coating. The drying and curing time (surface drying, hard drying) and the standardization of the material ratio (epoxy resin and curing agent) will affect the non-drying of the coating.

    4、地坪漆涂料的流变性及对涂装工艺的适应性,这对于地坪漆涂装的涂料尤其重要,涂料施工流平、防流挂、干燥时间控制是成膜关键。

    4. The rheology of floor paint and its adaptability to coating process are especially important for floor paint coating. The key to film formation is the leveling, anti-hanging and drying time control of the coating.