    引起环氧地坪颜色发白的5大原因与解决措施

    2018-10-20 07:51:14 无锡盛发地坪科技有限公司 阅读

    环氧地坪高质量、高价值,被应用到了很多领域。但应用得多了,环氧地坪就逐步暴露出了一些问题。业内有施工商反映,环氧自流平地坪完工后颜色不均衡,有些地方还会出现泛白的现象。业主追究起来,他们说不出所以然来,也没办法解决,实在让人头疼。为什么好端端的环氧地坪会泛白?出现泛白现象又该如何解决呢?下面,环氧地坪厂家小编就根据已有经验,为大家介绍导致这种情况出现的原因与相应解决措施。

    The epoxy floor is of high quality and high value, and has been applied to many fields. But with much application, the epoxy floor gradually exposes some problems. Some builders in the industry reflect that the color of the epoxy self-leveling floor is not balanced after completion, and some places will appear whitening phenomenon. Owners can not find out why they can't solve it. Why is the good epoxy floor whitening? How should we solve the problem of whitening? Below, the Royal Floor Bibliography on the basis of experience, for everyone to introduce the causes of this situation and the corresponding solutions. 

    原因1:漆膜干固时,由于有机溶剂沸点低,挥发快,挥发时会带走漆膜表面的温度,引起表面水汽凝结,出现一片片白雾,使漆膜失去光泽。

    Reason 1: When the film is dry and solidified, due to the low boiling point of organic solvents, volatilization is fast, volatilization will take away the surface temperature of the film, causing the surface of water vapor condensation, a piece of white fog, making the film lose luster. 

    解决措施:在施工前,留意施工环境的温度和湿度,可在施工中添加适量防潮剂或丁醇类憎水剂。

    Solutions: Before the construction, pay attention to the construction environment temperature and humidity, can be added in the construction of appropriate moisture-proof agent or butanol hydrophobic agent. 

    原因2:施工环境相对湿度>80%或漆膜、稀释剂中含水都会导致环氧地坪漆泛白。

    Reason 2: Relative humidity of construction environment > 80% or water content in paint film and thinner will lead to whitening of epoxy floor paint. 

    解决措施:将场地相对湿度控制在70%以下,并防止溶剂或空气带入水分。

    Solution: control relative humidity below 70% and prevent solvent or air from entering the water. 

    水性环氧地坪

    Waterborne epoxy floor

    美观的水性环氧地坪

    Beautiful waterborne epoxy floor 

    原因3:若在施工快干漆时使用过量的低沸点稀释剂就会造成漆膜发白的现象,严重的话还会引起多孔和细裂纹的问题。

    Cause 3: If the use of excessive low boiling point diluent in the construction of fast-drying paint will cause the phenomenon of whitening film, serious words will also cause porous and fine cracks. 

    解决措施:尽可能选用与快干漆配套的稀释剂,且注意稀释剂的用量。

    Solution: choose the thinner that is suitable for quick drying paint as far as possible, and pay attention to the amount of diluent. 

    原因4:施工环境空气流通不畅,且被涂物的温度低于室温。

    Reason 4: construction environment air circulation is not smooth, and the temperature of the coating is lower than room temperature. 

    解决措施:运用制热设备,提高室温;或引用热涂装工艺,在施工前将被涂件的温度提高至环境温度的110%。

    Solutions: Use heating equipment to raise the room temperature; or use thermal coating technology, will be coated before the construction of the temperature of 110% of the ambient temperature. 

    原因5:使用品质差、挥发快的稀释剂。

    Reason 5: use diluent with poor quality and fast volatilization. 

    解决措施:货比三家,选用质量好、挥发慢的稀释剂。

    Solution: goods three, choose good quality, slow volatile diluent. 

    环氧环氧地坪

    Epoxy floor

    美观的环氧地坪

    Beautiful epoxy floor 

    从上述内容我们不难看出,只要施工队在施工的过程中严格把握好每一个环节,熟悉环氧地坪泛白问题产生的原因并及时处理,环氧地坪泛白现象是可以预防的。因此,皇家地坪小编建议,在施工环氧地坪前,施工团队不妨多了解施工环氧地坪常出现的问题,防患于未然。

    From the above we can see that, as long as the construction team in the construction process to strictly grasp each link, familiar with the causes of whitening of epoxy floor and timely treatment, whitening of epoxy floor can be prevented. Therefore, the Royal Floor Bibliography suggested that before the construction of epoxy floors, the construction team may wish to know more about the construction of epoxy floors often appear problems, prevention in the future. 


    标签:   地坪 环氧地坪 环氧地坪漆 环氧地坪施工