    很多用久了环氧地坪漆可能会出现一些损坏,那么出现损坏的原因是什么呢?以及对它如何进行翻新呢?下面环氧地坪公司就来为大家解决这些疑惑吧!环氧地坪漆损坏的原因?工厂内装配的都是高档的机械设备,地面灰尘很容易附在或钻进这些设备内,而导致设备出现故障;这样即耽误工厂的生产,即造成订单的延误;又要花去公司很多经费来维修设备,对公司的损失是非常大的;如果车间地面未做处理,地面残破不堪,那么工厂的相关认证是无法通过的。普通水泥地面混凝土地面,一般使用数年后,在叉车的作用下地面全出现不同程度的翻砂、起尘现像,随着使用年限的增长,加上碳化、水侵蚀和风化的作用,环氧地坪表面会继续粉化,影响正常使用。

    Many epoxy floor paints may be damaged after a long time, so what is the cause of the damage? And how to renovate it? Now the epoxy floor company will solve these doubts for you! The reason for the damage of epoxy floor paints? The factory is equipped with high-grade machinery and equipment, and the dust on the ground is easy to attach. In or into these equipment, resulting in equipment failure; that is, delaying the production of the factory, that is, causing delays in orders; but also spend a lot of company funds to repair equipment, the loss of the company is very large; if the workshop floor is not processed, the ground is fragile, then the relevant factory certification is unable to pass. 。 After several years of general use, the concrete floor of ordinary cement ground appears sand-turning and dust-rising phenomena in varying degrees under the action of forklift trucks. With the increase of service life, together with the effects of carbonization, water erosion and weathering, the surface of the floor will continue to be powdered, affecting normal use. 环氧地坪漆地面:如果地面是采用薄涂材料施工,同时施工质量比较差,那么地面不到一年就会起皮,主要原因是该材料与地面粘结不牢固所致。

    Epoxy floor paint ground: If the ground is constructed with thin coating material and the construction quality is poor, the ground will peel in less than a year. The main reason is that the material is not firmly bonded to the ground.

    如果在一楼或地下室施工环氧材料,同时又没有做防水层,那么地面就会起泡或脱层,原因是在地下的水蒸汽被上面的环氧盖死,无法排除,就会产生起泡,同时就会慢慢产生脱层;

    If the epoxy material is constructed on the first floor or basement without waterproofing layer, the ground will foam or delaminate. The reason is that the water vapor in the ground is covered by the epoxy on the top, which can not be excluded, and the foaming will occur, at the same time, delamination will occur slowly.

    如果五金车间施工了环氧材料,那么地面很快就会被划痕和变脏,原因是环氧本身是树脂材料,不耐磨,不耐磨,所以很快就会被划痕和变脏。

    If the epoxy material is constructed in the hardware workshop, the ground will be scratched and dirty very quickly. The reason is that epoxy itself is a resin material. It is not wearable and wear-resistant, so it will be scratched and dirty very soon.

    金钢砂耐磨地面:起尘、起壳、空鼓、裂缝、坑凹等都与水泥混凝土地面情况相同;而退色则是由于金钢砂里面色粉的问题,如果色粉是采用比较差的材料,那么不到1年就会慢慢退色,特别是在室外受紫外线的照射,很快就会变色。

    Gold steel sand wear-resistant ground: dust, shelling, hollow drum, cracks, pits and so on are the same as cement concrete ground; and fading is due to the problem of color powder inside the gold steel sand. If the color powder is a relatively poor material, it will fade slowly in less than one year, especially when exposed to ultraviolet radiation outdoors, it will soon change. Color.


    环氧地坪漆的翻新:

    Renovation of epoxy floor paint:

    环氧防静电地坪翻新施工方案如下:

    The renovation construction scheme of epoxy anti-static floor is as follows:

    1、清理基层,用磨削机打磨水泥基层,然后用清水冲洗干净,晾干;清除旧环氧地坪。对于旧地坪要先使用专业的环氧消磨设备将其完全清除,这个第一步都是统一的,然后再根据不同的环氧地坪类型进行施工。

    1. Clean up the base, grind the cement base with a grinder, then rinse it with clean water and dry it; clear the old floor. For old floors, professional epoxy grinding equipment should be used to remove them completely. The first step is to unify them, and then to carry out construction according to different types of epoxy floors.

    2、刮涂环氧砂浆进行局部基层找平;清除油垢。如果地面有油污,要先将其清楚,再根据实际情况进行脱脂、脱油,确定表面干净后方可施工。

    2. Scraping epoxy mortar to leveling the local base; removing grease scale. If there is oil pollution on the ground, it should be clear first, then degrease and degrease according to the actual situation, and make sure that the surface is clean before construction.

    3、滚涂E152环氧封底漆(添加适量导电石墨)一遍,干燥4小时以上。

    3. Rolling coating of E152 epoxy sealing primer (adding appropriate amount of conductive graphite) once, drying for more than 4 hours.

    4、确定位置,铺设导电铜带网。

    4. Determine the location and lay conductive copper belt network.

    5、铺设导电汇流排并与导电铜网连接。

    5. Lay conductive busbar and connect with conductive copper network.

    6、按照要求设置接地装置。

    6. Set up grounding device according to requirement.

    7、地面刮涂防静电中间漆一至二遍,用于基层找平,干燥时间12小时以上,裂缝处理。材料和施工质量不好往往会造成地面裂缝产生,如果发现裂缝可以使用切割机把裂缝切成V形槽,然后灌入环氧砂浆使其平整即可。

    7. Scraping and painting anti-static intermediate paint on the ground once or twice, for leveling the base, drying time more than 12 hours, crack treatment. Poor material and construction quality often lead to ground cracks. If cracks are found, a cutting machine can be used to cut the cracks into V-shaped grooves and then pour epoxy mortar into them to make them flat.

    9、滚涂或刮涂防静电环氧面漆1至2遍,干燥时间24小时以上(对于自流平型的地面,本道工艺按照自流平地面做法进行,达到设计要求的最终厚度即可);

    9. Rolling or scraping anti-static epoxy topcoat 1 to 2 times, drying time is more than 24 hours (for self-leveling floor, this process is carried out according to the self-leveling floor method, the final thickness of the design requirements can be achieved);

    10、施工完毕后清理现场,养护七天。

    10. Clean up the site after completion of construction and maintain it for seven days.