欢迎光临无锡盛发地坪科技有限公司官网!【环氧地坪_防静电地坪_停车场地坪_耐磨地坪】材料生产,销售和施工的高新技术企业.

    示例图片三
    网站首页 > 新闻资讯 > 地坪知识

    验收时如何判断环氧自流平地坪漆的质量?

    2019-07-28 10:49:44 无锡盛发地坪科技有限公司 阅读

    环氧自流平地坪漆具有自动找平、耐磨、耐压的性能特点和高洁净、美观的环境要求,近几年来受到不少行业的好评和应用。环氧自流平地坪漆的性能是无可挑剔的,但是由于施工技术和涂料本身的质量问题,导致环氧自流平地坪漆的质量差异也非常显著。那么如何在验收时怎样判断环氧自流平环氧地坪漆的质量好坏,下面就简单来了解下:

    Epoxy self-leveling floor paint has the characteristics of automatic leveling, wear resistance and pressure resistance, and the requirements of high cleanliness and beautiful environment. It has been praised and applied by many industries in recent years. The performance of epoxy self-leveling floor paint is impeccable, but the quality difference of epoxy self-leveling floor paint is very significant due to the quality problems of construction technology and paint itself. So how to judge the quality of epoxy self-leveling floor paint when acceptance, the following is a simple understanding: 第一、表面状况。

    First, surface condition.


    环氧自流平环氧地坪是一种表面平滑、美观,具有优秀装饰效果的一种地坪,所以在验收的时候,要看清楚地坪表面是否平整、光亮可达镜面效果,且不能含有颗粒等杂物。

    Epoxy self-leveling floor is a kind of floor with smooth, beautiful surface and excellent decorative effect. Therefore, when acceptance, it is necessary to see clearly whether the surface of the floor is smooth and bright enough to achieve mirror effect, and it can not contain particles and other impurities.


    第二、硬度。

    Second, hardness.


    为了使地面有足够的耐磨性,许多客户都会要求地坪表面有一定的硬度。为了达到工业的使用要求,一般要求地坪的硬度大于2H。但是填料容易下沉的自流平固化后的硬度并不是太高,所以要选填料不易下沉的为佳。

    In order to make the floor wear-resistant enough, many customers will require a certain degree of hardness on the surface of the floor. In order to meet the requirements of industrial use, the hardness of floors is generally required to be greater than 2H. However, the hardness of self-leveling solidified fillers which are easy to sink is not too high, so it is better to choose fillers which are not easy to sink.


    第三、丰满度。

    Third, fullness.


    丰满度即是看地面的反光率是否能达到95%,是否够饱满。这个指标在以前是不受到重视的,但是随着社会的进步和人们的要求逐渐提高,这一项指标也渐渐变成了一项基本的技术要求。一般反射率达不到85%的都是不合格的。

    The fullness depends on whether the reflectivity of the ground can reach 95% or not. This index was not valued in the past, but with the progress of society and the increasing demands of people, this index has gradually become a basic technical requirement. Generally, those with reflectivity less than 85% are not qualified.


    标签:   环氧地坪 地坪 环氧地坪漆 环氧地坪施工 环氧地坪翻新