    解读环氧地坪漆是否涂层越厚越好?

    2019-07-02 09:00:38 无锡盛发地坪科技有限公司 阅读

    环氧地坪漆厂家温馨提醒:环氧地坪漆涂膜并不是越厚越好,只要按照环氧地坪漆施工工艺设计厚度要求即可,另外,施工时切忌一道涂层施工过厚,可以采取多遍涂刷的方法。许多消费者都认为环氧地坪漆漆膜越厚越好,当然不是那种理论上都达不到的厚度。但是实际上受环氧地坪漆固含量、干燥方式的影响,环氧地坪漆有其最小、推荐、最大的漆膜厚度,超过最大的漆膜厚度,一般并不会提升环氧地坪漆的性能、表面效果。甚至可能会影响环氧环氧地坪漆的性能,而且环氧环氧地坪漆的干燥性能影响非常明显。

    环氧地坪

    Warm reminder of epoxy floor paint manufacturers: epoxy floor paint coating is not the thicker the better, as long as according to the epoxy floor paint construction process design thickness requirements, in addition, construction should not be too thick a coating construction, you can take multiple brushing methods. Many consumers believe that the thicker the epoxy floor paint film, the better. Of course, it is not the thickness that can not be reached in theory. However, due to the influence of solid content and drying method of epoxy floor paint, epoxy floor paint has its minimum, recommended and maximum film thickness, which exceeds the maximum film thickness. Generally, it will not improve the performance and surface effect of epoxy floor paint. It may even affect the performance of epoxy floor paint, and the drying performance of epoxy floor paint is very obvious. 环氧地坪漆涂层结构

    Structure of Epoxy Floor Paint Coating环氧地坪漆漆膜过厚的影响:

    Effect of Epoxy Floor Paint Film Thickness:

    1、环氧地坪漆漆膜过厚最明显的就是浪费涂料,超过允许厚度的漆膜,并不会提升外观效果。

    1. Excessive thickness of epoxy floor paint film is the most obvious waste of paint. If the thickness exceeds the allowable thickness of paint film, it will not improve the appearance effect.2、环氧地坪漆漆膜过厚会对涂层的质量产生负面影响,影响环氧地坪的使用性能。

    2. Excessive thickness of epoxy floor paint film will have a negative impact on the quality of the coating and affect the performance of the epoxy floor.3、环氧地坪漆涂膜过厚,挥发性环氧地坪漆涂料的干燥就会不好,溶剂会残留在漆膜中,表层虽然已经干了,但是下层较软,容易引起涂层起泡与底材的结合力不好。对固化型环氧地坪漆涂料来说,则会产生内部缩孔,引起涂料开裂、剥落,这种现象特别容易在内角处发生。针孔也会因漆膜过厚而产生。

    3. If the epoxy floor paint is too thick, the drying of the volatile epoxy floor paint will be bad. Solvents will remain in the paint film. Although the surface layer has been dried, the lower layer is soft, which easily leads to poor adhesion between the foaming of the coating and the substrate. For cured epoxy floor paint, internal shrinkage will occur, causing cracking and peeling of the paint, which is particularly easy to occur at the inner corner. Pinholes can also occur because the paint film is too thick.