    什么因素导致环氧地坪出现色差发白和不干

    2019-06-28 10:46:31 无锡盛发地坪科技有限公司 阅读

    冬季环氧树脂油漆反映速度过慢,环氧树脂涂料主剂沉积。环氧地坪漆未充沛拌和均匀且硬化剂与空气反映发生白雾状,防止与前接缝处触摸距离太久,尽可能全部操作线一同施工。环氧树脂地坪施工后遭水侵入和在低温多湿之场合施工这两个情况也会发白。倒料在地面上,与前接缝处之触摸时间过久。尽量运用固定东西及加强施工人员施工熟练度。

    In winter, the reaction speed of epoxy resin paint is too slow, and the main agent of epoxy resin paint deposits. Epoxy floor paint is not fully mixed uniformly and the hardener and air reflect white fog, to prevent the contact distance with the front joint is too long, as far as possible all the operating lines are constructed together. Water intrusion after construction of epoxy floor and construction at low temperature and humidity will also bleach. Feeding on the ground and touching the front seam for too long. Make the best use of fixed things and strengthen the construction skillfulness of construction personnel. 基材外表处理不合格,外表残留油污或涂装底漆等,配方中采用了挥发性差的稀释剂或广州环氧地坪漆涂猜中混入油分。预涂底漆放置时间长也会致使慢干。

    Substrate surface treatment is not qualified, the appearance of residual oil or paint primer, etc. In the formulation, the use of poor volatility diluent or Guangzhou floor paint mixed with oil in painting guess. Pre-coated primer can also cause slow drying for a long time.


    因旧环氧地坪漆漆膜下附着大气污染物,双组分广州地坪漆涂料少加或未加固化剂。地坪底层水分含量高,一次涂施过厚或未干重涂,形成全体地坪漆涂层枯燥慢。

    Due to the air pollutants adhering to the old floor paint film, the two-component Guangzhou floor paint has little or no reinforcing agent. The bottom layer of the floor has high moisture content, and the coating is too thick or not dry re-coated at one time, which results in the dull and slow coating of all floor paints.