    环氧地坪漆施工粘度大的原因及解决办法

    2019-05-13 10:34:31 无锡盛发地坪科技有限公司 阅读

    环氧地坪漆施工时粘度不宜过大,否则就会出现施工困难的问题,下面环氧地坪漆厂家就给大家解答导致环氧地坪漆施工粘度大的原因及解决办法。环氧地坪漆施工粘度大的四个原因:1、不宜在气温过低的环境下施工,如果当时气温过低的话会直接出现黏度大现象。

    The viscosity of epoxy floor paint should not be too high during construction, otherwise there will be difficulties in construction. The following epoxy floor paint manufacturers will give you an answer to the causes and solutions of the high viscosity of epoxy floor paint construction. There are four reasons for the high viscosity of epoxy floor paint construction: 1. It is not suitable to construct in the environment of too low temperature. If the temperature is too low at that time, the high viscosity will appear directly. 2、在环氧地坪材料混合搅拌后,存放时间长,环氧地坪漆材料已反应就会发生黏度大现象。

    2. After mixing and stirring the floor materials, the epoxy floor paint materials will have high viscosity after long storage time.

    3、配料过程中加砂或加粉剂量过大,又没加溶剂从而导致黏度大现象。

    3. The excessive dosage of sand or powder and no solvent in the process of mixing lead to the phenomenon of high viscosity.

    环氧地坪漆施工粘度大解决办法

    Solution of high viscosity in epoxy floor paint construction:

    1、环氧地坪漆最佳施工温度为10-25℃,如果气温过低可以采取提高室内温度的方法。

    1. The optimum construction temperature of epoxy floor paint is 10-25 C. If the temperature is too low, the method of increasing indoor temperature can be adopted.

    2、减少混合搅拌后的存放时间,每次配料要在半小时之内施工完毕。

    2. Reduce the storage time after mixing and mixing, each batching should be completed within half an hour.

    3、减少砂的加入量,如果粘度大可以适当的添加稀释剂。

    3. Reduce the amount of sand added, if the viscosity is high, the diluent can be added appropriately.