    施工过后环氧地坪漆厚度检测方法介绍

    2019-05-06 08:24:55 无锡盛发地坪科技有限公司 阅读

    由于环氧地坪漆的种类比较多,根据所选择的环氧地坪漆施工工艺的不同,环氧地坪漆的厚度也各不相同,而厚度直接决定着环氧地坪漆的使用寿命(参考《环氧地坪漆一般能用多长时间》),涂膜厚度不达标会影响环氧地坪漆的性能,导致涂膜过早的失效,影响环氧地坪工程的使用寿命。膜厚度超出标准则会造成工程成本的增加,影响溶剂的挥发和完全干燥。因此,为了保证环氧地坪漆的施工质量,施工后需要对环氧环氧地坪漆的厚度进行检测,具体检测方法如下:

    Because there are many kinds of epoxy floor coatings, the thickness of epoxy floor coatings varies according to the different construction technology. The thickness directly determines the service life of epoxy floor coatings (refer to "How long can epoxy floor coatings generally last"). The performance of epoxy floor coatings will be affected by the thickness of the coatings not up to the standard, leading to premature failure of the coatings and affecting the floor. The service life of the flat project. If the film thickness exceeds the standard, the engineering cost will increase and the volatilization and drying of solvent will be affected. Therefore, in order to ensure the construction quality of epoxy floor paint, it is necessary to test the thickness of epoxy floor paint after construction. The specific detection methods are as follows: 环氧地坪漆厚度的检测必须在涂膜完全干燥后,使用专用的干膜测厚仪进行测定,一般可以使用破坏性仪器和卡尺,检测的时候选择的测量点要具有代表性,但由于检测具有破坏性,测量点应选择边角等不影响外观的地方取样和检查。

    The thickness of epoxy floor paint must be measured by a special dry film thickness gauge after the film is completely dried. Destructive instruments and calipers can be generally used. The selected measuring points should be representative. However, due to the destructive testing, the measuring points should be sampled and inspected in places that do not affect the appearance, such as edges and corners.

    环氧地坪漆涂膜厚度的要求:

    Requirements for film thickness of epoxy floor paint:

    环氧地坪漆涂膜厚度所有测定点结果的平均值应大于等于规定干膜厚度的90%,不能超过规定最大干膜厚度的10%.当合格率低于80%,需全面补涂;合格率为80%-90%,应根据情况做局部补涂;当涂膜厚度超过规定最大干膜厚度的10%时,应设法解决。

    The average value of the film thickness of epoxy floor paint at all measuring points should be greater than 90% of the prescribed dry film thickness and not more than 10% of the prescribed maximum dry film thickness. When the qualified rate is less than 80%, it needs to be fully repaired; the qualified rate is 80%-90%, local repairing should be done according to the situation; when the film thickness exceeds 10% of the prescribed maximum dry film thickness, solutions should be found.


    标签:   地坪 环氧地坪 环氧地坪漆 环氧地坪施工