欢迎光临无锡盛发地坪科技有限公司官网!【环氧地坪_防静电地坪_停车场地坪_耐磨地坪】材料生产,销售和施工的高新技术企业.

    示例图片三
    网站首页 > 新闻资讯 > 地坪知识

    环氧地坪施工基础地面不平整怎么解决?

    2019-04-30 09:06:02 无锡盛发地坪科技有限公司 阅读

    环氧地坪漆具有整体无接缝、耐腐蚀、防尘防水、维护方便和强度高、耐磨损等优点,表面光亮美观,能达镜面效果。如果基础地面不平整,做出来的环氧地坪漆在光亮反光的情况下就会出现凹凸不平的现象,影响环氧地坪漆的整体美观性。因此,在环氧地坪漆施工前需要检测基础地面的平整度,如果地面不平,就需要先进行处理。

    Epoxy floor paint has the advantages of seamless, corrosion resistance, dust-proof and waterproof, convenient maintenance, high strength and wear resistance. It has a bright and beautiful surface and can achieve mirror effect. If the base floor is uneven, the resulting floor paint will appear uneven in the case of bright reflection, affecting the overall aesthetics of epoxy floor paint. Therefore, before the construction of floor paint, it is necessary to check the flatness of the foundation ground. If the ground is uneven, it needs to be treated first. 

    基础地面平整度检测方法:

    Testing method of foundation ground roughness:

    一般来说,环氧地坪漆要求基面平整度在2m范围之内,采用2m的靠尺进行测量,并且落差不能超过2mm。

    Generally speaking, epoxy floor paint requires the base surface smoothness to be within 2m range, measured by 2m gauge, and the drop can not exceed 2m M.

    基础地面不平整解决方法:

    Solutions to foundation ground irregularity:

    a、落差小于5mm

    A. The drop is less than 5 mm

    1、打磨。使用打磨机或洗地打磨机配置金刚磨头进行基面打磨,将高出点打磨到与低点平行。

    1. Grinding. The base surface is polished with a diamond grinder equipped with a grinder or a floor washing grinder, and the high point is polished parallel to the low point.

    2、刮砂。环氧砂浆地坪适用于这种方法。在中涂施工时,在刮砂这道工序时,以光磊环氧树脂中涂与石英砂进行混合,填充混凝土基面基面,实现找平的效果。

    2. Scraping sand. Epoxy mortar floor is suitable for this method. During the construction of intermediate coating, in the process of sand scraping, a mixture of quartz sand and epoxy resin is used to fill the base of concrete to achieve leveling effect.

    b、落差大于5mm

    B. A drop greater than 5 mm

    混凝土基面平整度在5mm以上,那用打磨机进行找平,或用环氧树脂中涂刮砂找平成本将是巨大的,而且砂层厚度过高会对地坪漆性能造成一定影响。这时候可以在落差在5mm以上的混凝土基面,重新施工3-5cm的水泥砂浆层,重新原浆收光,找平最好。

    If the smoothness of concrete base is more than 5 mm, the cost of leveling by grinding machine or scraping sand in epoxy resin will be enormous, and the excessive thickness of sand layer will affect the performance of floor paint. At this time, we can rebuild the cement mortar layer of 3-5 cm on the concrete foundation with a drop of more than 5 mm, and the original slurry can be re-lightened to find the best level.


    标签:   地坪 环氧地坪 环氧地坪漆 环氧地坪施工