    环氧地坪漆施工出现凹陷原因及解决方案,施工面上出现多像针刺过而留下的痕迹状态,涂膜出现圆形凹窝,这种施工现象在验收时是不合格的那么我们如何找到环氧地坪施工后出现凹陷的原因,找到原因后又怎么去解决呢,小迪今天给大家提供环氧地坪施工出现凹陷原因以及环氧地坪施工出现凹陷解决。环氧地坪漆在施工过程中会出现像针刺过一样的痕迹状态,涂膜出现圆形凹窝,这种施工现象在验收时是不合格。

    Causes and solutions of depression in epoxy floor paint construction, like the traces left by needling on the construction surface, circular depression in the coating film, this construction phenomenon is not qualified in acceptance, then how can we find the reasons for depression after epoxy floor construction, and how to solve it after finding the reasons? Xiaodi today provides you with the construction of epoxy floor depression. Cause and settlement of sag in epoxy floor construction. During the construction of epoxy floor paint, there will be traces like needles, and circular pits appear in the film. This construction phenomenon is not qualified at the time of acceptance. 一、环氧地坪漆在施工过程中出现凹陷是什么原因所导致?

    1. What causes the depression of epoxy floor paint in the construction process?

    (1)环氧地坪漆涂膜表面不均,涂膜未固化前有水滴在膜上,底层有油或胶,构成洼陷;

    (1) The surface of the floor paint is uneven. Before the film is cured, there are water droplets on the film and oil or glue on the bottom, which form a depression.

    (2)环氧地坪漆涂抹基面无打磨过润滑;环氧地坪漆工程.

    (2) No abrasion or lubrication on the base surface of floor paint; epoxy floor paint engineering.

    (3)溶剂沸点低涂膜流平差。

    (3) Flow adjustment of film with low boiling point of solvent.

    (4)夏季施工人员留下的汗珠滴在未固化涂膜上,往往也会造成凹陷。

    (4) In summer, sweat droplets left by builders on uncured coatings often cause depressions.

    (5)基面层的密实性不均;填料分散不足;

    (5) The compactness of the base layer is not uniform, and the filler is not dispersed enough.

    二、环氧地坪施工出现凹陷解决方案

    2. Solution to Sag in Epoxy Floor Construction

    (1)施工现场避免任何水分触摸没有固化的涂膜;底层要打磨粗化要清洁净;环氧地坪漆厂.涂料和溶剂或稀释剂选用要配套,要根据施工现场环境合理选用。

    (1) Avoid any water touch on the construction site without curing the coating; the bottom should be polished and coarsened to be clean; the epoxy floor paint factory. Paint and solvent or diluent selection should be matched, and reasonable selection should be based on the construction site environment.

    (2)更换性能合格的涂料,施工时防止汗水接触未固化的。

    (2) Replacement of qualified coatings to prevent perspiration from contacting uncured coatings during construction.

    (3)加强施工人员的技术培训;施工时防止任何水分接触材料,未固化前。

    (3) Strengthen the technical training of construction personnel; prevent any water contact materials during construction, before solidification.