    (1)为使环氧地坪漆涂料的施工达到良好的效果,对于尚未找平的地面,应首先施工水泥找平层以进行找平处理。土建方找平时,在水泥初凝时,用专业地面机械对地面进行磨平处理。经过基层处理再涂装的环氧地坪漆的表面会更平整、光亮,使用寿命也会提高。

    (1) In order to achieve good results in the construction of epoxy floor paint, cement leveling layer should be first applied to leveling the ground that has not yet been leveled. When constructing the cement, the civil engineers usually use the professional ground machinery to grind the ground. The surface of epoxy floor paint after base treatment and re-coating will be smoother and brighter, and its service life will also be improved.

    (2)待水泥层干燥后(大约28天),用打磨机对地面进行整体打磨处理,使其表面平整,水泥毛细孔全部敞开。

    (2) After the cement layer is dried (about 28 days), the whole ground is polished with a grinder to make the surface smooth and the cement capillary holes open.

    (3)对于有油污(食用油、机油)的基层,先用表面处理剂喷洒于用水冲湿的地表面,反复擦洗,直到无油污为止。如何控制环氧地坪漆涂料施工质量

    (3) For the base layer with oil contamination (edible oil, engine oil), the surface treatment agent is sprayed on the surface wetted with water and scrubbed repeatedly until there is no oil contamination. How to control construction quality of floor paint

    (4)对于碱性太大(PH>8)的基层,先用稀盐酸或者稀醋酸进行中和处理,然后用清水冲洗。

    (4) For the base layer with too high alkalinity (PH > 8), neutralize it with dilute hydrochloric acid or acetic acid, then rinse it with clean water.

    (5)对于潮湿地面,通过吸水、擦干,太阳、灯照,热风机吹烘,使其含水率达到施工要求。

    (5) For wet ground, the water content can reach the construction requirement by absorbing water, drying, sunshine, lamp illumination and hot air blower.

    (6)对于有旧漆膜的地面(如金刚砂环氧地坪、旧漆膜地面),先用机械铲除旧油漆,然后对局部不良情况进行处理,同时对地面打毛,以清除不牢固的旧水泥层及金刚砂表面,并且形成粗毛面,从而提高新涂层的附着力。

    (6) For the surface with old paint film (such as diamond floor and old paint film floor), the old paint is first removed mechanically, and then the local bad conditions are treated. At the same time, the ground is groomed to remove the unstable old cement layer and diamond surface, and form rough surface, so as to improve the adhesion of the new coating.

    (7)对于较深的伸缩缝,须先用彩色弹性胶填充到低于地平面约1~2mm的高度,然后用快干硬油漆腻子刮平;对于已填了沥青的伸缩缝,要将缝中的沥青铲平到低于地平面1~2mm的深度,然后用快干硬油漆腻子刮平,防止返色。

    (7) For deep expansion joints, it is necessary to fill them with colour elastic glue at a height of about 1-2 mm below the ground surface, and then scrape them with quick-drying hard paint putty; for those expansion joints filled with asphalt, the asphalt in the joints should be flattened to a depth of 1-2 mm below the ground surface, and then scraped with quick-drying hard paint putty to prevent discoloration. 